Casting defects are unwanted irregularities that occur in cast products due to improper mould design, poor material control, or incorrect process parameters. Common casting defects include blowholes, shrinkage cavities, cold shuts, and misruns, and they can be reduced by proper mould preparation, controlled pouring temperature, adequate venting, and correct gating design.
In this article:
Casting Defects and Their Remedies
Casting defects are imperfections in the cast product caused by improper mould design, melting, pouring, or solidification.
1. Blow Holes
Description
- Smooth, round cavities inside or on the surface of casting
- Caused by entrapped gases
Causes
- High moisture in moulding sand
- Poor permeability
- Gas dissolved in molten metal
- Turbulent pouring
Remedies
- Reduce moisture content in sand
- Improve sand permeability
- Proper venting of mould
- Degas molten metal
- Smooth and controlled pouring
2. Porosity
Description
- Small, distributed gas holes throughout casting
Causes
- Hydrogen or gas absorption
- Inadequate degassing
- High pouring temperature
Remedies
- Proper degassing
- Use dry moulds and cores
- Control pouring temperature
- Use vacuum casting if required
3. Shrinkage Cavity
Description
- Irregular internal cavities formed during solidification
Causes
- Improper feeding of molten metal
- Absence or improper size of riser
- Poor solidification control
Remedies
- Provide proper risers
- Use chills to control solidification
- Proper gating system design
- Directional solidification
4. Misrun
Description
- Incomplete filling of mould cavity
Causes
- Low pouring temperature
- Slow pouring rate
- Poor fluidity of metal
- Thin sections
Remedies
- Increase pouring temperature
- Increase pouring rate
- Improve metal fluidity
- Modify casting design
5. Cold Shut
Description
- A line or seam where two metal streams meet but do not fuse
Causes
- Low metal temperature
- Oxidation of molten metal
- Improper gating design
Remedies
- Increase pouring temperature
- Improve gating system
- Reduce turbulence
- Ensure proper metal flow
6. Hot Tears (Hot Cracks)
Description
- Cracks formed during solidification at high temperature
Causes
- Restricted contraction
- Sharp corners in casting
- Poor mould collapsibility
Remedies
- Provide fillets and rounded corners
- Improve mould collapsibility
- Proper riser placement
- Uniform cooling
7. Inclusions
Description
- Non-metallic materials trapped inside casting
Causes
- Slag, sand, or oxide inclusions
- Turbulent metal flow
- Poor metal cleaning
Remedies
- Use slag traps
- Proper fluxing and skimming
- Smooth metal flow
- Clean mould cavity
8. Sand Drop
Description
- Lumps of sand fall into molten metal creating cavities
Causes
- Weak mould strength
- Improper ramming
- Excessive metal velocity
Remedies
- Proper sand ramming
- Improve sand strength
- Reduce metal pouring speed
9. Scab
Description
- A rough, raised area on casting surface
Causes
- Expansion of mould sand
- High moisture content
- Weak mould surface
Remedies
- Reduce sand moisture
- Use proper sand additives
- Improve sand strength
10. Metal Penetration
Description
- Metal enters sand interstices, causing rough surface
Causes
- Coarse sand
- High pouring temperature
- Low mould hardness
Remedies
- Use finer sand
- Increase mould hardness
- Reduce pouring temperature
11. Flash
Description
- Thin excess metal at mould joints
Causes
- Poor mould alignment
- Improper clamping
- High metal pressure
Remedies
- Proper mould assembly
- Adequate clamping
- Reduce pouring pressure
Summary Table
| Defect | Main Cause | Remedy |
|---|---|---|
| Blow holes | Gas entrapment | Venting, degassing |
| Porosity | Dissolved gas | Degassing |
| Shrinkage | Lack of feeding | Risers, chills |
| Misrun | Low fluidity | Higher temp, faster pour |
| Cold shut | Poor fusion | Better gating |
| Hot tears | Restricted contraction | Fillets, collapsibility |
| Inclusions | Slag/sand | Fluxing, slag traps |
| Sand drop | Weak mould | Better ramming |
| Scab | Sand expansion | Control moisture |
| Penetration | Coarse sand | Finer sand |
| Flash | Poor alignment | Proper clamping |
Other courses: